Full brims, mouse ears, with glue, without glue, higher bed temperature, lower bed temperature, flat base, concentric cutout base - whatever I try, I seem to be getting wank adhesion, major warping, and ultimately this shitshow.
Dry PLA, warm room, no draught, plate cleaned with IPA. I’m going to fucking punch this thing in its stupid fucking face.
Edit: Prevailing advice very much seems to be to bust out the Fairy liquid and give it a good scrub, so I’ll try that. It’s a Kobra Neo 2 so is auto-levelling, so I can’t piss around with any of that stuff (as far as I know). Another quick question while I think about it, does everyone always print onto the bed at ~60°C? Because Orca Slicer’s default for a textured PEI plate is 45°C, which seems mad. I think I tried it once and it was shite so turned it back up to 60.
empireOfLove2@lemmy.dbzer0.comEnglish
17·2 days ago- verify actual bed and print nozzle temp using IR or contact probe. Thermistors can die and cause too low a temp.
- fully wash bed with soap and water, not just IPA.
- try a different spool or brand of filament. Sometimes whole spools are just formulated badly and it won’t ever adhere right. I’ve tossed a few spools that wouldn’t ever print correctly no matter the settings.